Transition joints from stranded Al conductors to solid Cu conductors 10 mm² / 8 AWG (e.g. Excel, Excelett). Two crimps are needed for both Al (crimp sequence see image) and Cu.
Cat. No. | Area mm² | CuAWG/MCM | Solid AlArea mm² | Solid AlAWG/MCM | Stranded AlArea mm² | Stranded AlAWG/MCM | d | d1 | D | D1 | L | s |
---|---|---|---|---|---|---|---|---|---|---|---|---|
AKS16-10S | 10 | 8 AWG | 25 | 4 AWG | 16 | 6 AWG | 5.9 | 4.5 | 13 | 7 | 64.5 | 29 |
AKS25-10S | 10 | 8 AWG | 35 | 2 AWG | 25 | 4 AWG | 6.8 | 4.5 | 13 | 7 | 64.5 | 29 |
AKS35-10S | 10 | 8 AWG | 50 | 10 AWG | 35 | 2 AWG | 8.5 | 4.5 | 20 | 7 | 86 | 45 |
AKS50-10S | 10 | 8 AWG | 70 | 20 AWG | 50 | 1/0 AWG | 9.6 | 4.5 | 20 | 7 | 86 | 45 |
AKS70-10S | 10 | 8 AWG | 95 | 40 | 70 | 2/0 AWG | 11.3 | 4.5 | 20 | 7 | 86 | 45 |
AKS95-10S | 10 | 8 AWG | 120 | 250 | 95 | 4/0 AWG | 12.5 | 4.5 | 25 | 7 | 101 | 60 |